@article { author = {Akbarpoor, Iman and Resalati, Hossein}, title = {The Effect of Different Concentrations of Cellulase Enzyme on Optical and Physical Properties of ONP Deinked Pulp}, journal = {Iranian Journal of Wood and Paper Industries}, volume = {2}, number = {1}, pages = {1-15}, year = {2012}, publisher = {Iranian Scientific Association of Wood and Paper Industries}, issn = {2008-9066}, eissn = {2423-3242}, doi = {}, abstract = {Enzymes are protein molecules with complex structures that accelerate the biochemical reactions. Activity of these chemical compounds is accomplished at limited range of pH, temperature and concentration. In this study, the effects of different concentrations of cellulose enzyme were investigated on deinking of old newsprint. Old newsprint (ONP) was repulped at 5% consistency for 10 minutes in disintegrator with total revolution number of 26500. Enzymatic treatments of recycled ONP pulp were done under constant conditions (10% consistency,treatment time of 15 minutes, pH range of 5-5.5) at different cellulose concentrations of 0.025, 0.05, 0.1 and 0.2% (based on oven-dry waste paper). The optical and physical properties of the standard paper (60g/m2) made at different concentrations of cellulose were evaluated in comparison with control pulp (untreated ONP pulp with cellulase). Overall, the results achieved by comparison the optical properties of the paper produced indicated that using cellulase in deinking of ONP led to increase the brightness and the yellowness and decrease the opacity. The brightness was improved to a maximum level of 47.5 ISO %, but the yellowness was decreased to a minimum level of 11.3 ISO %, while the brightness reduced and the yellowness increased at higher concentrations than 0.05% cellulase. The highest opacity of 99.3 ISO % was achieved using 0.1% cellulase even higher than control pulp. The results gained by comparison the physical properties of the paper showed that using cellulase resulted in decrease of paper calliper, air resistance and density and improve the freeness of pulp}, keywords = {: cellulase Enzyme,Deinking,Old Newsprint,Optical Properties,physical properties}, title_fa = {تاثیر غلظت های مختلف آنزیم سلولاز بر ویژگی های نوری و فیزیکی خمیرکاغذ روزنامه مرکب زدایی شده}, abstract_fa = {آنزیم‌ها مولکول‌های پروتئینی با ساختار پیچیده می باشند که واکنشهای زیست شیمیایی را شتاب می‌دهند. فعالیت این ترکیبات شیمیایی در دامنه محدودی از pH ، دما و غلظت صورت می گیرد. در این پژوهش تأثیر غلظت های مختلف آنزیم سلولاز در مرکب زدایی کاغذ روزنامه باطله مورد بررسی قرار گرفت. کاغذ روزنامه باطله در شرایط درصد خشکی 5% به مدت زمان10 دقیقه در دستگاه پراکنده ساز با دور26500 به خمیرکاغذ تبدیل شد. تیمار آنزیمی خمیرکاغذ روزنامه بازیافتی در شرایط ثابت ( درصد خشکی10%، زمان تیمار 15 دقیقه، محدوده 5/5-5 pH ) در غلظت های مختلف 025/0، 05/0، 1/0، 2/0 درصد آنزیم سلولاز (بر پایه وزن خشک کاغذ باطله) انجام گرفت. ویژگی های نوری و فیزیکی کاغذهای استاندارد( g/m260) ساخته شده در غلظت های مختلف آنزیم سلولاز در مقایسه با خمیرکاغذ شاهد(خمیرکاغذ تیمار نشده با سلولاز) ارزیابی شدند. نتایج حاصل از مقایسه ویژگی های نوری کاغذهای ساخته شده نشان داد که آنزیم سلولاز در مرکب زدایی کاغذ روزنامه باطله در مقایسه با خمیرکاغذ شاهد در مجموع منجر به افزایش روشنی و زردی و کاهش ماتی کاغذ شده است. با افزایش غلظت آنزیم سلولاز از 025/0 به 05/0 درصد، روشنی به بیشینه میزان 5/47 درصد ایزو بهبود یافت و زردی کاغذ به کمینه میزان 03/11 درصد ایزو کاهش یافت. این در حالی است که در غلظت های بیشتر از 05/0 درصد سلولاز، روشنی کاهش یافته و به زردی کاغذ افزوده شد. بیشترین ماتی 3/99 درصد ایزو با استفاده از 1/0 درصد آنزیم سلولاز حتی بیشتر از خمیرکاغذ شاهد به‌دست آمد. نتایج حاصل از مقایسه ویژگی های فیزیکی کاغذهای ساخته شده نشان داد که استفاده از آنزیم سلولاز در مرکب زدایی کاغذ روزنامه باطله در مقایسه با خمیر کاغذ شاهد منجر به کاهش ضخامت، مقاومت به عبور هوا و دانسیته کاغذ و بهبود درجه روانی خمیرکاغذ شده است.}, keywords_fa = {آنزیم سلولاز,مرکب زدایی,کاغذ روزنامه باطله,ویژگی های نوری,ویژگی های فیزیکی}, url = {https://www.ijwp.ir/article_11429.html}, eprint = {https://www.ijwp.ir/article_11429_1fe06032aaaa84e0981f24cd39bb600c.pdf} } @article { author = {Gholamian, Hadi and Tarmian, Asghar and Doust hosseini, Kazem and Azadfallah, Mohammad}, title = {The Effect of Clear Paints, Nanozycofil and Nanozycosil on Water Absorption and Contact Angle of Poplar Wood}, journal = {Iranian Journal of Wood and Paper Industries}, volume = {2}, number = {1}, pages = {17-26}, year = {2012}, publisher = {Iranian Scientific Association of Wood and Paper Industries}, issn = {2008-9066}, eissn = {2423-3242}, doi = {}, abstract = {In this research, the effect of nano-zycosil, nano-zycofil, acid catalyzed lacquer and nitrocellulose lacquer and polyester on improving the water absorption and contact angle of wood was investigated. Some boards were prepared from the sapwood of poplar (P.nigra). They were dried based  on T6E3 schedule and some specimens were cut according to EN 927-5 standard (20 × 70 × 150 mm).  They were coated and immersed with the nano particles and clear paints.  The clear paint- and nanoparticles-coated samples were dried in laboratory environment and in an oven at the temperatures of 1032°c, respectively. After drying process, the water absorption of the samples was measured after 2, 24, 72, 168 h immersion. The contact angle of samples was measured after 1 and 10 seconds. The results revealed that the pattern of water absorption for the paints and nanoparticles is different. The samples coated with combined acid catalyzed lacquers and nitrocellulose lacquers and those coated with nanozycosil had the highest resistance to water absorption. The greatest contact angle was observed for the samples coated by nanozycosil.}, keywords = {water absorption,Contact angle,Nanozycosil,Nano-zycofil Acid catalyzed lacquers,Polyster}, title_fa = {بررسی اثرگذاری رنگ های شفاف و نانوذرات زایکوفیل و زایکوسیل بر زاویه تماس و جذب آب در چوب صنوبر}, abstract_fa = {در این تحقیق تاثیر نانو ذرات زایکوسیل و زایکوفیل و رنگ‌های پلی‌استر و سیلروکیلر در بهبود مقاومت به جذب آب و افزایش زاویه تماس چوب مورد ارزیابی قرار گرفت. برای این منظور، تخته‌های تهیه شده از برون چوب صنوبر (P.nigra) برابر برنامه چوب‌خشک‌کنی با کد 3E6T خشک شدند و سپس نمونه‌هایی برابر با استاندارد 5-927 EN (20 × 70 × 150 میلیمتر) تهیه شد. نمونه‌ها با تیمارهای مختلفی از نانو ذرات و رنگ‌های شفاف یاد شده پوشش‌داده شدند. نمونه‌های پوشش‌داده شده با رنگ‌های شفاف در شرایط آزمایشگاهی و نمونه‌های پوشش‌داده شده با نانو ذرات در درون آون در دمای °c‌2±103 خشک شدند. پس از خشک‌کردن، جذب آب نمونه ها پس از 2 ،24 ،72 و168 ساعت غوطه‌وری در آب مقطر و میزان زاویه تماس آن ها در ثانیه اول و دهم اندازه‌گیری شد. نتایج نشان داد که برای هر یک از پوشش‌ها، الگوی تغییرات جذب آب و زاویه تماس متفاوت بود. نمونه‌های پوشش‌داده شده با ترکیب دو رنگ سیلروکیلر و نیم‌پلی‌استربراق و نمونه‌ های پوشش‌داده شده با نانو ذرات زایکوسیل بیشترین مقاومت را به جذب آب از خود نشان دادند. بیشترین زاویه تماس در نمونه پوشش داده شده با نانو زایکوسیل مشاهده شد.   }, keywords_fa = {جذب‌آب,زاویه تماس,نانو زایکوسیل,نانو زایکوفیل,سیلروکیلر,نیم‌پلی‌استربراق}, url = {https://www.ijwp.ir/article_11430.html}, eprint = {https://www.ijwp.ir/article_11430_93876ca16069fbddb35bc72944c5912d.pdf} } @article { author = {Talae, Aysona and Karimi, Ali naghi and Ebrahimi, Ghanbar and Mirshokrai, Ahmad}, title = {Comparative Study of Heat Treated Beech Wood in Hot Water and Steam Mediums}, journal = {Iranian Journal of Wood and Paper Industries}, volume = {2}, number = {1}, pages = {27-38}, year = {2012}, publisher = {Iranian Scientific Association of Wood and Paper Industries}, issn = {2008-9066}, eissn = {2423-3242}, doi = {}, abstract = {Heat treatment of wood is an effective method to improve the dimensional stability and durability against biodegradation. Heat treatments of beech wood in 2 different mediums (hot water and steam) at 180ºC were compared by physical, mechanical and anatomical properties. Mass loss in hydrothermally treated wood was higher than hygrothermally treated specimens. Mechanical properties (MOR and MOE) were decreased in both mediums, but strength loss was higher for hygrothermal treated samples. Anatomical changes were investigated by means of a light microscopic analysis. Beech was sensitive to collapse of the vessels in both mediums. In treated beech, radial cracks were observed near the rays both in hydro and hygrothermal treatments. Depletion of extractives on the cell walls and deformation of libriform fibers near the vessels were also observed.}, keywords = {Hydrothermal,hygrothermal treatment,Beech,Density,swelling,strength loss,anatomy}, title_fa = {بررسی مقایسه ویژگی‌های فیزیکی، مکانیکی و ساختاری چوب راش پس از تیمار گرمایی در دو محیط فراگیر آب و بخار آب}, abstract_fa = {در این پژوهش تیمار گرمایی چوب راش در دو محیط فراگیر متفاوت (آب و بخارآب) در دمای Cº180 انجام شده است. سپس ویژگی‌های فیزیکی، مکانیکی و ساختاری آزمونه‌های تیمار شده در این دو فرایند مقایسه شدند. کاهش چگالی خشک در آزمونه‌های تیمار‌شده به روش آب‌گرمایی بیشتر از آزمونه‌های تیمار‌شده به روش بخار‌گرمایی بود. چوب راش در اثر تیمار آب‌گرمایی واکشیدگی کمتر و پایداری ابعاد بیشتری نسبت به تیمار بخار‌گرمایی پیدا کرده بود. ویژگی‌های مکانیکی (MOR, MOE) در هر دو تیمار کاهش یافت ولی کاهش مقاومت در اثر تیمار بخار‌گرمایی بیشتر بود. تغییرات ساختاری آزمونه‌ها با میکروسکوپ نوری بررسی شدند. چوب راش تیمار‌شده حساس به چین خوردگی درونی (Collapse) آوندها در هر دو محیط فراگیر آب و بخار آب بود. ترک‌های شعاعی در اطراف اشعه چوبی در هر دو تیمار دیده شدند. رسوب مواد استخراجی روی جدار سلولی و تغییر ‌شکل لیف‌های دوکی شکل (لیبریفرم) نیز در حواشی اشعه‌ها دیده شدند.  }, keywords_fa = {تیمار آب‌گرمایی,تیمار بخار‌گرمایی,چوب راش,خواص فیزیکی,خواص مکانیکی,خواص ساختاری}, url = {https://www.ijwp.ir/article_11431.html}, eprint = {https://www.ijwp.ir/article_11431_4d5d95b6d4d48531b99391a269688568.pdf} } @article { author = {Dalvand, Mosayeb and Maleki, Sadegh and Gholamian, Hadi and Tarmian, Asghar}, title = {Measuring the Drying Kinetics and Mass Transfer Coefficients of Hornbeam Wood (Carpinus betulus) from Nooshahar Region}, journal = {Iranian Journal of Wood and Paper Industries}, volume = {2}, number = {1}, pages = {39-51}, year = {2012}, publisher = {Iranian Scientific Association of Wood and Paper Industries}, issn = {2008-9066}, eissn = {2423-3242}, doi = {}, abstract = {In this research, drying kinetics and mass transfer coefficients (permeability and diffusion) of hornbeam wood (Carpinus betulus) from Nooshahar region were investigated. For this purpose, several boards with two nominal thicknesses of 2.5 an 5 cm were prepared from a freshly cut log. The boards were dried inside a laboratory kiln at the dry bulb temperature of 40°C and relative humidity of 50% to the final moisture content of 6%. The pattern of moisture loss, thermal diffusion, final moisture gradient along the board thickness, transverse permeability and diffusion coefficients were then measured. The results showed that by increasing of board thickness, the rate of moisture loss decreased, particularly in the hygroscopic range and the moisture gradient increased, but the thermal diffusion was not affected. The transverse permeability and diffusion coefficient of hornbeam wood was 2.91 × 10 -19 m 2 and 3.29 × 10 -9 m 2s-1, respectively. Overall, it can be concluded that due to low transverse permeability coefficient of hornbeam wood, this species is difficult to be impregnated in common wood preservation process. In contrast, due to low diffusion coefficient, hornbeam wood is recommended for applications where high resistant to water vapor diffusion is required.  }, keywords = {Hornbeam wood,Permeability,diffusion,Drying kinetics}, title_fa = {بررسی تعیین سینتیک خشک شدن و ضرائب انتقال جرم گونه چوبی ممرز(Carpinus betulus) از منطقه نوشهر}, abstract_fa = {در این بررسی سینتیک خشک شدن و ضرائب انتقال جرم (ضریب نفوذپذیری و ضریب انتشار)چوبگونه ممرز(Carpinusbetulus) از منطقه نوشهر مورد ارزیابی قرار گرفت. برای این منظور، از گرده‌بینه تازه بریده شده تخته‌هایی با دو ضخامت اسمی 5/2و 5 سانتی‌متر تهیه شد و سپس در یک خشک‌کن آزمایشگاهی در دمای ° c40 و رطوبت نسبی 50 درصد تا رطوبت نهایی 6 درصد خشک شدند. الگوی خروج رطوبت، انتشار دما، گرادیان نهائی رطوبت در راستای ضخامت تخته‌ها و ضریب نفوذپذیری و انتشار عرضی تخته‌ها اندازه‌گیری شد. نتایج نشان داد که با افزایش ضخامت تخته‌ها، نرخ خروج رطوبت به ویژه در دامنه جذب و دفع (هیگروسکپیک) کاهش یافته و شیب گرادیان رطوبت بیشتر شده ولی فرایند انتشار دما تحت تاثیر قرار نگرفت. ضریب نفوذپذیری و ضریب انتشار عرضی چوب ممرز به ترتیب برابر با 2m 19-10×91/2 و                           1-s 2 m9-10× 29/3 اندازه‌گیری شد. بنابراین با توجه به ضریب نفوذپذیری عرضی کم چوب ممرز، این گونه در کلاسۀ گونه‌های چوبی سخت اشباع در صنعت حفاظت چوب قرار می‌گیرد. در مقابل به دلیل ضریب انتشار عرضی کم آن، چوب ممرز برای کاربردهایی که نیاز به مقاومت بالا در مقابل انتشار بخار آب است، پیشنهاد می‌شود.}, keywords_fa = {چوب ممرز,ضریب نفوذپذیری,ضریب انتشار,(سینتیک) خشک‌شدن}, url = {https://www.ijwp.ir/article_11441.html}, eprint = {https://www.ijwp.ir/article_11441_0bf4d8ce1d7488dd20cb2bdca065b721.pdf} } @article { author = {Hosseinpour, Reza and J.Latibari, Ahmad and Tajdini, Azhang and Sepide dam, M.Javad and Hossein, M.Ali}, title = {Investigation on the Influence of Chemical Treatment Time and Temperature on the Properties of CMP from Colza Stem}, journal = {Iranian Journal of Wood and Paper Industries}, volume = {2}, number = {1}, pages = {533-62}, year = {2012}, publisher = {Iranian Scientific Association of Wood and Paper Industries}, issn = {2008-9066}, eissn = {2423-3242}, doi = {}, abstract = {The influence of chemical treatment time and temperature on production of chemi-mechanical pulp from Colza stem is studied. Three treatment times (15, 30 and 45 minutes) and two treatment temperatures (125 and 145 °C) were investigated. Chemical charge as 4% NaOH and 8% Na2SO3 as was kept constant. Accepted pulp yield varied between 53.8%  and 63% and the total yield was measured between 57.6% and 68.9%. The residual lignin in lower yield pulp was 19% and higher yield pulp was 20.4%. Holocellulose content of pulps varied between 72.5%- 74% and freeness was between 520-590 ml CSF. Fiber classification using Bauer-McNett procedure showed that the average fiber length of unrefined pulp is between 0.6-0.7 mm, and the fine content (P100) is between 9% and 10.4%, Pulp freeness was reduced from original value of 520 to 590 ml CSF to about 300 ml CSF as pulps were refined in PFI mill applying 500 revolutions. The unrefined pulp strength including tensile index, burst index and tear index were measured as 15.48- 26.13 N.m/g, lower than 1 kPa.m2/g and 2.91- 4.34 mNm2/g respectively. All the indices after refining in PFI mill using 500 revolution were increased to 19.74-35.19 N.m/g, Max. 1.70 kPa.m2/g and 3.21- 4.68 mNm2/g respectively}, keywords = {}, title_fa = {بررسی تاثیر زمان و دمای فراوری شیمیایی (پخت) بر ویژگی‎های خمیر کاغذ CMP از ساقه کلزا}, abstract_fa = {ساخت خمیر کاغذ شیمیایی- مکانیکی از پسماند کلزا با هدف بررسی تاثیر زمان و دمای مرحله فراوری شیمیایی بر کیفیت خمیر کاغذ از ساقه کلزا انجام گرفته است. متغیرهای فراوری شیمیایی شامل دو دمای 125 و 145 درجه سلسیوس و سه زمان 15، 30 و 45 دقیقه و با مصرف 4٪ هیدروکسید سدیم و 8٪ سولفیت سدیم در یک محفظه پخت تحت فشار انجام گرفت. بازده قابل قبول بین کمینه 8/53٪ تا بیشینه 63٪ بود و بازده کل بین 6/57٪ تا 9/68٪ تعیین شد. میزان لیگنین باقی مانده در خمیر کاغذ با بازده کمتر معادل 19٪ و برای  بازده زیادتر برابر با 4/20٪ بود. هولوسلولز خمیر کاغذ نیز بین 5/72٪ تا 74٪ و درجه روانی اولیه بین 520 تا 590 میلی لیتر استاندارد کانادایی اندازه گیری شده است، که پس از 500 دور پالایش در پالایشگر PFI به حدود 300 میلی لیتر استاندارد کانادایی رسید. طبقه بندی الیاف خمیر کاغذ پالایش نشده با استفاده از غربال های بوئر- مکنت انجام شد.  میانگین طول الیاف بین 6/0 تا 7/0 میلی متر بود و میزان نرمه های عبور کرده از غربال 100 مش بین 9 تا 4/10% اندازه گیری شد. شاخص مقاومت در برابر کشش خمیر کاغذ پالایش نشده بین 47/15 تا 14/26 N.m/g اندازه گیری شده که پس از پالایش به 74/19 تا 19/35  N.m/g افزایش یافت. شاخص مقاومت در برابر پاره شدن خمیر کاغذهای پالایش نشده بین 91/2 تا 34/ 4   /g2 m.Nm متغیر بوده که پس از پالایش به 21/3 تا 68/ 4 /g2 m.Nmافزایش یافته است. شاخص مقاومت در برابر ترکیدن خمیر کاغذهای پالایش نشده کمتر از یک /g2kPa.m بوده است که پس از پالایش به بیشینه 70/1/g2kPa.m افزایش یافت.}, keywords_fa = {کلزا,خمیر کاغذ شیمیایی- مکانیکی,بازده,میانگین طول الیاف,ویژگی مقاومتی}, url = {https://www.ijwp.ir/article_11442.html}, eprint = {https://www.ijwp.ir/article_11442_744d48e3d2f29de472d5e6356cd353bd.pdf} } @article { author = {Pourabbasi, Sara and Kord, Behrouz}, title = {Investigation on the Effect of Chemical Foaming agent and Wood Flour content on Mechanical Properties, Density and Cell morphology of HDPE/EVA/ Wood Flour Hybrid Foamed Composites}, journal = {Iranian Journal of Wood and Paper Industries}, volume = {2}, number = {1}, pages = {63-80}, year = {2012}, publisher = {Iranian Scientific Association of Wood and Paper Industries}, issn = {2008-9066}, eissn = {2423-3242}, doi = {}, abstract = {In this research, the effects of chemical foaming agent and wood flour content on cell morphology, density and mechanical properties of HDPE/EVA/ Wood Flour hybrid foamed composites were investigated. For this aim, composites were prepared via melt mixing in an internal mixer, then foamed using single-stage batch foaming method. Then mechanical properties such as flexural strength, flexural and tensile modulus and density were measured. Morphology of the samples was also evaluated by scanning electron microscopy (SEM). The results of this study have indicated that the flexural strength, flexural and tensile modulus and density increases with the increase of wood flour content. However, with addition of chemical foaming agent content and EVA content, mechanical properties and density of foamed composites decreased. Moreover, wood fiber acted as nucleating agents that substantially reduced cell size and increased cell density. In addition, EVA plays an important role in foaming process by increasing the melt viscosity of the polymer matrix, in a way that samples with higher content of EVA have the highest cell density and the lowest cell size.}, keywords = {Chemical Foaming Agent,Morphology,EVA,Batch foaming Method,Hybrid Foamed Composites}, title_fa = {بررسی اثر میزان ماده کف زای شیمیایی و آرد چوب بر ویژگیهای مکانیکی، چگالی و ریخت شناسی چندسازه سبک شده هیبریدی پلی اتیلن سنگین/ اتیلن وینیل استات/آرد چوب}, abstract_fa = {در این تحقیق تأثیر میزان ماده کف‌زای شیمیایی و آرد چوب  بر ویژگیهای مکانیکی، چگالی و ریخت شناسی چندسازه سبک شده هیبریدی پلی اتیلن سنگین/ اتیلن وینیل استات/ آرد چوب مورد بررسی قرار گرفت. برای این منظور، چندسازه‌ها با استفاده از فرآیند اختلاط در یک مخلوط کن داخلی تهیه و سپس به روش تک مرحله‌ای (Batch) فوم شدند. سپس خواص مکانیکی شامل مقاومت خمشی، مدول خمشی و کششی و چگالی اندازه‌گیری شدند. ریخت شناسی نمونه‌ها نیز با عکسبرداری با میکروسکوپ الکترونی(SEM) مورد ارزیابی قرار گرفت. نتایج نشان داد با افزایش میزان آرد چوب، مقاومت خمشی، مدول خمشی و کششی و چگالی افزایش یافت. در حالی‌که با افزایش میزان ماده کف زای شیمیایی و EVA، خواص مکانیکی و چگالی چندسازه‌های فوم شده کاهش یافت. همچنین آرد چوب به عنوان عامل هسته‌گذار عمل کرده و منجر به کاهش اندازه سلولی و افزایش چگالی سلولی گشت. از طرفی، EVA  با افزایش گرانروی مذاب ماتریس پلیمری، نقش مهمی را در فرآیند فوم شدن ایفاء نمود. به گونه‌ای که نمونه‌های دارای میزان EVA بیشتر، دارای بیشترین میزان چگالی سلولی و کمترین اندازه سلولی گشتند.  }, keywords_fa = {ماده کف‌زای شیمیایی,ریخت شناسی,EVA,فوم کردن به روش (Batch),چندسازه سبک شده هیبریدی}, url = {https://www.ijwp.ir/article_11443.html}, eprint = {https://www.ijwp.ir/article_11443_cc80b0ba1afdacbb2d611c10f6410efb.pdf} } @article { author = {Mehdinia, Meysam and Tabarsa, Taghi and Sadeghian, M.Mehdi}, title = {Investigation the Plywood Manufacturing of Paulownia (paulownia tomentosa) with Urea and Phenol Formaldehyde Adhesives}, journal = {Iranian Journal of Wood and Paper Industries}, volume = {2}, number = {1}, pages = {81-89}, year = {2012}, publisher = {Iranian Scientific Association of Wood and Paper Industries}, issn = {2008-9066}, eissn = {2423-3242}, doi = {}, abstract = {In recent years, the plywood and veneer industry of Iran has undergone negative growth due to shortage of proper diameter logs and also lack of innovative technologies for the use of low-diameter logs; Moreover, demands for lignocelluloses products has been growing as a consequence of  significant increase in population and expansion of construction Industry, especially in major cities. Hence, it is necessary to cultivate fast-growing species. For this purpose four logs of paulownia (120 cm length and 55 cm diameter) were prepared from the Gorgan shast Kalate forests and then transported to Kosar factory in order to prepare veneers. Produced layers were transferred to the wood laboratory of Gorgan university. Then plywood was manufactured from paulownia species on the basis of the standard 3210 of ISIRI (Institute of Standards and Industrial Researches of Iran) and common tests of plywood were made. The results showed that the mechanical properties of manufactured boards were upper than with standards defined by ISIRI and the physical properties of those manufactured with urea formaldehyde glue were lower than standards which can be considered as negative properties; Albeit, they were not significant and can be disregarded}, keywords = {Plywood,lack of wood,population growth,pautonia,Paulownia,Urea and Phenol formaldehyde}, title_fa = {ارزیابی ساخت تخته لایه از گونه پالونیا با بهره‌گیری از دو نوع چسب اوره و فنل فرمالدهید}, abstract_fa = {در سال های اخیر صنعت تخته لایه و روکش به علت کمبود گرده بینه های با قطر مناسب و همچنین نبود فناوری‌های نوین برای بهره‌گیری از گرده بینه های کم قطر در کشور، دارای رشد منفی بوده است. این در حالی است که با افزایش چشمگیر جمعیت و در نتیجه گسترش ساختمان سازی بویژه در کلان شهرها، تقاضا برای مصرف فرآورده های لیگنوسلولزی روز به روز در حال افزایش است. بنابراین به نظر می رسد که بهره‌گیری از چوب های تولیدی در دوره های بهره برداری کوتاه مدت (زراعت چوب) برای تأمین ماده اولیه مورد نیاز صنایع یادشده امری اجتناب ناپذیر می باشد. بنابراین در این راستا تخته لایه هایی از گونه پالونیا ساخته شد و خواص فیزیکی و مکانیکی آن مورد ارزیابی قرار گرفت. برای این منظور 4 گرده بینه از گونه پالونیا (با طول 120 و قطر55 ساتی متر) از جنگل های شصت کلاته گرگان تهیه و برای لایه گیری به کارخانه کوثر در گنبد منتقل شد. سپس لایه های تهیه شده (با ضخامت 4 میلی متر) به آزمایشگاه علوم و صنایع چوب دانشگاه گرگان منتقل شد و تخته لایه های مورد نظر برابر استاندارد 3210 موسسه استاندارد و تحقیقات صنعتی ایران تهیه و آزمایش‌های مربوطه بر روی آنها انجام شد. نتایج حاصله نشان داد خواص مکانیکی تخته های ساخته شده بالاتر از حد استاندارد بوده و در مورد خواص فیزیکی تنها برای نمونه های تولید شده با چسب اوره فرمالدهید کمتر از حد مجاز بود که البته این اختلاف معنی دار نبود و میتوان آن را در حد استاندارد در نظر گرفت.}, keywords_fa = {تخته لایه,کمبود چوب,رشد جمعیت,گونه های تند رشد,پالونیا,چسب های اوره و فنول فرمالدهید}, url = {https://www.ijwp.ir/article_11444.html}, eprint = {https://www.ijwp.ir/article_11444_ca048b9acbf0181f553d6fdf6471146f.pdf} } @article { author = {Seraian, A.Reza and Shoub chari, Hossein}, title = {Investigation on the Fiber Biometry and Chemical Compounds of Bast and without Bast Stalk of Cotton Stalk Sahel Variety}, journal = {Iranian Journal of Wood and Paper Industries}, volume = {2}, number = {1}, pages = {91-101}, year = {2012}, publisher = {Iranian Scientific Association of Wood and Paper Industries}, issn = {2008-9066}, eissn = {2423-3242}, doi = {}, abstract = {In order to determine the fiber dimensions, physical and chemical properties of the bast and without bast stalk of Sahel-Variety of cotton stalk, required samples were prepared and studied. The results showed that fiber and lumen diameter and  cell wall thickness of  without bast stalk fibers were greater than those of bast fibers, while bast fibers were longer. Thus, this fibers can be classified as short and medium length fibers respectively.Data showed that the Length/ Diameter ratio and Runkle ratio of the bast fibers were greater than those of without bast stalk fibers, and flexibility coefficient in without bast stalk fibers was greater. Stalk with higher diameter had less bast proportion.Oven-dried density and swelling and shrinkage values of thicker stalks were greater than those of thinner ones, but apparent and basic densities,as well as porosity in thinner stalks were higher. Chemical Properties of bast and without bast stalk were respectively as follow: cellulose 39.27% and 48.3%,lignin 23.93% and 21.89% ,extractives 6.06% and 3.23% , ash content 6.36% and 1.85% ,one percent sodium hydroxide solubility 48.35% and 21.275% and hot water solubility19.48% and 9.68%.These indicate that without bast stalk fibers are more suitable than bast fibers for pulp production, but bast fibers are preferred in terms of fiber length.}, keywords = {Cotton Stalk Sahel Variety,Bast,without Bast Stalk,fiber dimensions,Chemical compounds}, title_fa = {بررسی زیست سنجی الیاف و ترکیبات شیمیایی پوست و ساقه بدون پوست پنبه رقم ساحل}, abstract_fa = {به منظور تعیین ابعاد الیاف، ویژگی های فیزیکی و ترکیبات شیمیایی پوست و ساقه بدون پوست پنبه رقم ساحل نمونه های مورد نظر تهیه و مورد بررسی قرار گرفتند. نتایج نشان داد که قطر، قطر حفره سلولی و ضخامت دیواره سلولی الیاف ساقه پنبه بدون پوست نسبت به الیاف پوست بیشتر بود، در حالی که پوست الیاف بلندتری داشت. با توجه به نتایج بدست آمده می توان گفت که الیاف ساقه پنبه بدون پوست و پوست به ترتیب در ردیف الیاف کوتاه و متوسط قرار می گیرند. ضرایب درهم رفتگی و نسبت رانکل در الیاف پوست بیشتر بودند در حالی که ضریب انعطاف پذیری در الیاف ساقه پنبه بدون پوست بیشتر از الیاف پوست بود. ضمن اینکه با افزایش قطر ساقه پنبه میزان پوست نسبت به ساقه آن کاهش می یابد. ساقه های با قطر زیادتر در مقایسه با ساقه های کم قطرتر، چگالی خشک بیشتر و همکشیدگی و واکشیدگی حجمی بیشتری داشتند، اما چگالی بحرانی و ظاهری همراه با میزان تخلخل در ساقه های کم قطرتر بیشتر بود.میزان ترکیبات شیمیایی پوست و ساقه بدون پوست این رقم به ترتیب به شرح زیر تعیین شدند: سلولز 27/39% و 38/48%، لیگنین 93/23% و 89/21%، مواد استخراجی 06/6% و 23/3%، میزان خاکستر36/6% و 85/1%، مواد قابل حل در سود سوزآور یک درصد 35/48% و 275/21% و مواد قابل حل در آب داغ 48/19% و 68/9% . اگرچه ساقه پنبه بدون پوست از لحاظ ویژگی های شیمیایی برای خمیرسازی نسبت به پوست آن مطلوب تر است اما پوست از جنبه بلندی الیاف برتر می باشد.}, keywords_fa = {: ساقه پنبه رقم ساحل,پوست,ساقه بدون پوست,ترکیبات شیمیایی}, url = {https://www.ijwp.ir/article_11445.html}, eprint = {https://www.ijwp.ir/article_11445_cf4edae4b4afa577f8b24e6f02c68a96.pdf} } @article { author = {Eslah, Farnaz and Enayati, A.Akbar and Faezipour, Mehdi and Tajvidi, Mehdi}, title = {Investigation the Effect of Increasing Board Density and Amount of UF Resin on Particleboard Properties}, journal = {Iranian Journal of Wood and Paper Industries}, volume = {2}, number = {1}, pages = {103-112}, year = {2012}, publisher = {Iranian Scientific Association of Wood and Paper Industries}, issn = {2008-9066}, eissn = {2423-3242}, doi = {}, abstract = {In order to investigation the effect of increasing board density and amount of UF resin on particleboard properties, this study was carried out. .Regarding two variable parameters: board density at three level (520, 620 and 720Kg/m3) and percentage of UF resin (6, 7, and 8%),one layer particleboards with16mm nominal thickness were manufactured. Physical and mechanical properties such as MOR, MOE, IB and thickness swelling (after 24 hours immersion in water) were measured. The results showed that with increase in board density from 520 to 720 Kg/m3, MOR and MOE were increased and dimensional stability were improved. But increase in board density had no significant effect on IB. The results of contour plots showed that manufacturing boards with density of 600-650 Kg/m3and 6% UF resin, all of mechanical properties were maintained in standard specified limits related to those boards and using adequate amount of water resistant materials will Cause improving of thickness swelling after 24 h immersion}, keywords = {Particleboard,Poplar,Resin content,Board density,Physical and mechanical properties,contour plots}, title_fa = {ارزیابی میزان اثر گذاری افزایش تراکم جرم تخته و میزان چسب بر روی ویژگی های تخته خرده چوب}, abstract_fa = {برای ارزیابی میزان اثرگذاری افزایش تراکم جرم تخته و میزان چسب بر روی ویژگی های تخته خرده چوب ، با در نظر گرفتن دو عامل متغیر تراکم جرم تخته در سه سطح 520، 620 و 720 کیلوگرم بر متر مکعب و میزان چسب در سه سطح 6، 7 و 8 درصد، تخته خرده چوب یک لایه با ضخامت 16 میلی متر ساخته شد. ویژگی های مکانیکی و فیزیکی شامل مقاومت و مدول خمشی، چسبندگی درونی واکشیدگی ضخامت پس از 24 ساعت غوطه وری در آب اندازه گیری شدند. نتایج نشان داد که با افزایش تراکم جرم تخته از 520 به 720 کیلوگرم بر متر مکعب مقاومت و مدول خمشی تخته ها افزایش یافته و پایداری ابعاد آن ها بهبود می یابد. اما افزایش تراکم جرم اثر معنی داری بر مقاومت چسبندگی درونی تخته‌ها نداشت. افزایش مصرف چسب از 6 تا 8 در صد بر همه ویژگی های فیزیکی و مکانیکی تاثیر معنی داری داشته و منجر به بهبود آنها شد. نقشه های اثرگذاری های متقابل که با نرم افزار 15minitab رسم شدند نشان دادند که تخته های با تراکم جرم 650-600 کیلوگرم بر مترمکعب و 6 درصد چسب، دارای ویژگی های مکانیکی بالاتر از حد نصاب میزان تعیین شده توسط استاندارد مربوطه بوده ضمن اینکه افزایش جزئی واکشیدگی ضخامت تخته ها را نیز می توان با مصرف میزان معمول مواد ضد آب جبران کرد.}, keywords_fa = {تخته خرده چوب,صنوبر,چسب اوره فرم آلدهید,دانسیته تخته,خواص فیزیکی- مکانیکی,نقشه اثرات متقابل}, url = {https://www.ijwp.ir/article_11446.html}, eprint = {https://www.ijwp.ir/article_11446_ba9ac006a31d16900a763e98a24d0f6f.pdf} } @article { author = {D.Hosseini, Kazem and Mahdinia, Meysam and Farhid, Elham and Elyasi, Abdollah}, title = {Investigation the Potential Replacement of the Old Corrugated Container (OCC) and Poplar Wood Flour Instead of Wheat Flour such as Urea-formaldehyde Adhesive Filler in the Plywood Industry}, journal = {Iranian Journal of Wood and Paper Industries}, volume = {2}, number = {1}, pages = {115-125}, year = {2012}, publisher = {Iranian Scientific Association of Wood and Paper Industries}, issn = {2008-9066}, eissn = {2423-3242}, doi = {}, abstract = {Considering the value and importance of wheat flour in our country, replacement of a new type of filler instead of wheat flour in glue combination in plywood industry is necessary. In this study the possibility of using wood flour of poplar and OCC (old corrugated container) fiber as filler in the combination of urea formaldehyde glue has been studied. The plywood was manufactured from Poplar species (in core of plywood) and Hornbeam veneer (in back and face of plywood) on the basis of the standard 3210 of ISIRI (Institute of Standards and Industrial Researches of Iran) and the physical and mechanical properties of experimental plywood were measured. The results of statistical analysis of variance and Least Significant Difference (LSD) showed that Mechanical and physical properties of samples made with fine OCC were more than that of control samples (the Samples made with wheat flour filler). The results also showed physical and mechanical properties of plywood increase by adding 10 to 15 percent of OCC to adhesive}, keywords = {: plywood,Urea formaldehyde,wheat flour,poplar wood flour,old corrugated container}, title_fa = {بررسی قابلیت جایگزینی پسماند الیاف کارتن کهنه(OCC) و آرد چوب گونه صنوبر به جای آرد گندم به‌عنوان پر کننده چسب اوره فرمالدهید در صنعت تخته لایه}, abstract_fa = {با توجه به ارزش و اهمیت تغذیه‌ای آرد گندم در کشور ضرورت جایگزینی نوع جدیدی از پر کننده به جای آن در ترکیب چسب احساس می شود. در این تحقیق امکان استفاده از الیاف حاصل از کارتن کهنه (old corrugated container) و آرد چوب گونه صنوبر به عنوان پر کننده در ترکیب چسب اوره فرمالدهید مورد بررسی قرار گرفته است. تخته لایه های حاصل(تخته سه لایه) در این تحقیق از لایه های صنوبر(در قسمت میانی) و لایه های ممرز (در لایه سطحی) برابر استاندارد 3210 موسسه استاندارد و تحقیقات صنعتی ایران تهیه و ویژگی های فیزیکی و مکانیکی آن مورد ارزیابی قرار گرفت. نتایج حاصل از مقایسه آماری تجزیه واریانس و کمترین اختلاف معنی دار(LSD) نشان داد که مقاومت های مکانیکی و فیزیکی مربوط به نمونه های ساخته شده با پر کننده OCC ریز بیش از نمونه های شاهد (نمونه های ساخته شده با پر‌کننده آرد گندم) و دیگر نمونه ها بود. همچنین نتایج نشان داد مصرف 10 تا 15 درصد از OCC موجب افزایش خواص فیزیکی و مکانیکی تخته ها می‌شود.}, keywords_fa = {تخته لایه,پر کننده,اوره فرمالدهید,آرد گندم,آرد چوب صنوبر,الیاف کارتن کهنه}, url = {https://www.ijwp.ir/article_11447.html}, eprint = {https://www.ijwp.ir/article_11447_674f87d654328bfc5ea8b4c6a992100f.pdf} }